Hi all,

I am currently faced with a requirement from a customer to meet C5-M corrosion resistance on a die cast aluminium alloy. However it has to also have a RAL colour finish.

The component is quite small, i would describe as lunch box size, which i understand is quite small for a heavy duty paint system & will result in areas of high DFT.


Are there any alternative protections i can use to meet this? I am thinking of anodisation with a final powder coat, but is this something that is feasible?

All ideas/suggestions would be appreciated

Thanks
Gareth
 
Replies continue below

Recommended for you

Anodizing is possible, and so it powdercoating. You should preheat the casting (temperature below powdercoating curing point) to de-gas it (entrapped gas porosity is a common condition with high pressure die casting), which will prevent bubbles in the powdercoating.
 