Looking for a source to purchase C-350 Maraging steel in Australia.

Thanks, Ken
 
Replies continue below

Recommended for you

Quantities?

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
If you are looking for bar you might try

Allegheny Technologies International Inc.
Australia Branch
Suite 501, 1 Princess Street
Kew 3101, Victoria
Australia Phone: 011-61-3-9205-9622
Fax: 011-61-3-9853-9066

Alvac makes the product, they might be able to point you to a distributor.

= = = = = = = = = = = = = = = = = = = =
Rust never sleeps
Neither should your protection
 
Small quantities!! 16mm OD bar by 300mm would be ample.

Thanks for the contact Edstainless, rang them and looks like it does need to be imported. anyone have some lying around??