Hello, I am working on a byspeed 4.4kw MMC operating system.
What are the recommended piercing modes for stainless steel and aluminum?
Is it better using normal piercing or pulsed piercing mode to protect the lens more?
Is a dilema I have and I'm curious what you guys recommend.
 
Replies continue below

Recommended for you

you can only change this on the part preparation software (bysoft)
 