Can anyone tell me what the main advantages would be of having a 7%Cr martensitic material instead of BW10?
I am aware they both have reasonable wear resistance, and suspect 7%Cr is more expensive.
Is 7%Cr a more 'castable' material?
Is there a big difference when it comes to having them in high temperature service?
I am aware they both have reasonable wear resistance, and suspect 7%Cr is more expensive.
Is 7%Cr a more 'castable' material?
Is there a big difference when it comes to having them in high temperature service?