Dear Friends,
We have some stock butterfly valves purchased from a company in Korea. The company is completely closed now. The name plates of the valves has no value on pressure value @ 100 Deg F. Our client informed us to punch the pressure value as per the standard & deliver the vale to them. I referred the standard & have taken the below pressure values. Please help me if I am correct:
A216 WCB body with PTFE seat - Pressure rating @ 100F is 285 PSI based on ASME B16.34. Is this correct
A351 CF8 body with PTFE seat - Pressure rating @ 100F is 275 PSI based on ASME B16.34. Is this correct
B148 C95800 body with PTFE seat - Pressure rating @ 100F is 195 PSI based on ASME B16.24. Is this correct
A126 CLB body with NBR seat - I do not know the Pressure rating @ 100F. Can any one help me
We have some stock butterfly valves purchased from a company in Korea. The company is completely closed now. The name plates of the valves has no value on pressure value @ 100 Deg F. Our client informed us to punch the pressure value as per the standard & deliver the vale to them. I referred the standard & have taken the below pressure values. Please help me if I am correct:
A216 WCB body with PTFE seat - Pressure rating @ 100F is 285 PSI based on ASME B16.34. Is this correct
A351 CF8 body with PTFE seat - Pressure rating @ 100F is 275 PSI based on ASME B16.34. Is this correct
B148 C95800 body with PTFE seat - Pressure rating @ 100F is 195 PSI based on ASME B16.24. Is this correct
A126 CLB body with NBR seat - I do not know the Pressure rating @ 100F. Can any one help me