Hi,

Can we weld a 2.5"x1" reducer to a 1"x.5" reducer and then to a 3/4" tubing with butt weld prep at its ends.

All the reducers are ASME B16.9 butt weld fittings.
Any advise is much appreciated.
 
Replies continue below

Recommended for you

Draw your configuration ((to scale! and with exact proposed part geometries and weld prep's)) and upload the sketch/"print to pdf" file.

I "think" I understand what you "think" you want to do/are planning on doing, but I'm not saying anything until I actually understand your situation.
 
The preparation you've suggesting will probably not pass a radiograph unless you do the correct end prep on the 0.5" NPS pipe end that you intend to butt-weld to the 3/4" tubing. But if you match the tube OD and ID on the 0.5" butt welding end, I don't see a problem with what you're proposing to do.

I wouldn't join tubing to pipe in this way unless there was a good reason not to have a tube fitting there. Instead I'd butt- or socket-weld a tube fitting to the pipe, but that's just my preference.
 
I agree with moltenmetal. Use a tube fitting.

I work in the nuclear industry, and we will typically use socket weld fittings on pipe that is 2" and smaller, and we almost always use Swagelok tube fittings.

If I were doing the design, I would cap the 2-1/2" pipe with a buttweld cap, and then use a 3/4" sockolet. The sockolet could be on the side of the pipe as a branch connection, or you could attach it to the end of the pipe on the cap. Then use a Swagelok adapter (part number -1210-1-12W) that has a male 3/4" pipe end (to be socket welded into the sockolet) and a 3/4" tubing compression connection.
 