davidbeach
Electrical
Does anybody have any good data on busway zero sequence impedances? I'm looking for conclusive information on low voltage busway, copper or aluminum bus bars, with an aluminum housing. Conrad St. Pierre's book, table B-8, has a set of Z0/Z1 ratios for steel housing. Those ratios have a fairly wide range, do not reflect the differences between R0/R1 and X0/X1, and are for steel rather than aluminum housing.
The impedance data on the web sites of the major manufacturers does not address this issue, at least not directly. They do provide the housing resistance, presumably there would also be some reactance but at a much lower level than the case with steel housing.
Thanks,
David Beach
The impedance data on the web sites of the major manufacturers does not address this issue, at least not directly. They do provide the housing resistance, presumably there would also be some reactance but at a much lower level than the case with steel housing.
Thanks,
David Beach