Anybody know any good correlations (pref. with a litterature ref.) for a aproximation of the heat loss from a buried pipe where the value should be a heat resistance coefficient R or equivalent (so that the value can be incorporated in a standard U estimation).

I know the one that is often seen lifted from the "Transactions of the American Institute of Electrical Engineers, The temperatures of buried Caples and Pipes" Volume 68, Part I 1949" that are commenly used. But i have been told that it is inaccurate at low pipe temperatures.

Best Regards

Morten Andersen
 
Replies continue below

Recommended for you

My reference is "Cold Climate Utilities Manual" by the Canadian Society for Civil Engineering. Original equations/development likely from other sources.

For bare pipe buried in soil, depth z to center, Rp is pipe radius, k is soil conductivity, Ts is temperature at surface, Tz is temperature at pipe depth, Tw is temperature of fluid in pipe;

Rg=[arccosh (z/Rp)]/2*pi*k;

and q=(Tw-Ts)/Rg ---heat loss per unit length
 