Hi, I am new to the aerospace industry and wonder if anyone can assist me with a question related to 'burn through'. As I understand it, the issue of burn through can be, as an example, applicable to galley equipment. In the event of extreme heat or exposure to a flame, the rate of burn through a galley monument or partition wall becomes very important.

Can anyone give me a summary of the burn through issue or let me know where I can find information please,

Thank you,
Jeff
 
have you looked at the FAA's AC on this ?

another day in paradise, or is paradise one day closer ?
 
There is also the SMOKE, FIRE AND FUMES IN TRANSPORT AIRCRAFT document from the Royal Aeronautical for general back ground.

Plus there are quite a number of Cabin fire related reports on FAA website (they seem to have moved since I last looked).
 
Many thanks for your replies Gentlemen !
 
IF unfamiliar... Some useful info...

FAA AC20-178 Flammability Testing of Aircraft Cabin Interior Panels After Alterations

FAA AC23-2 Flammability Tests

FAA AC25.853-1 Flammability Requirements for Aircraft Seat Cushions

DOT/FAA/AR-00/12 Aircraft Materials Fire Test Handbook

SAE ARP695 Galley System Design and Installation Criteria

ASE AS1426 App II Standard Galley System Specification - Appendix II - 20.0 Data Requirements and Procedures

SAE AS6453 Fire Containment Cover - Design, Performance, and Testing Requirements [Cargo ULD covers to prevent burn-thru by smothering]

Regards, Wil Taylor

o Trust - But Verify!
o We believe to be true what we prefer to be true. [Unknown]
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation,Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", Homebuiltairplanes.com forum]
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top