Due to overhual of exchanger we found that, hard scale inside tubes and most the tubes are blugged and have Bulging.
we tried to clean it by 10000 psi water jet but still the tubes are blugged and difficult to clean it.
Therefor, we can't use eddy current test(to check on tube thickness and their intgrities) due to blugging
The design pressure of the tube is 7.0 kg/cm2.
fluid is sea water
Design temp. is 60 C
operating temp. is 39.6
opertaing pressureis 1 kg/cm2
Tube material is copper nickel( C7060T )
Are there any method of cleaning or temperary & permenant solution?
Note:
it can't be cleaned by chemical, because that may lead to tube corrosion
we tried to clean it by 10000 psi water jet but still the tubes are blugged and difficult to clean it.
Therefor, we can't use eddy current test(to check on tube thickness and their intgrities) due to blugging
The design pressure of the tube is 7.0 kg/cm2.
fluid is sea water
Design temp. is 60 C
operating temp. is 39.6
opertaing pressureis 1 kg/cm2
Tube material is copper nickel( C7060T )
Are there any method of cleaning or temperary & permenant solution?
Note:
it can't be cleaned by chemical, because that may lead to tube corrosion