Jan 11, 2008 #1 rheim Structural Joined Jan 16, 2007 Messages 40 Location US Where can I find information about how to repair a built-up plywood beam, such as glue type, nailing patterns etc? Thanks for help Roland
Where can I find information about how to repair a built-up plywood beam, such as glue type, nailing patterns etc? Thanks for help Roland
Jan 12, 2008 #2 csd72 Structural Joined May 4, 2006 Messages 4,574 Location GB I wouldnt rely on glue. Proprietary glulams e.t.c. are verified by testing, not calculations. Upvote 0 Downvote
Jan 12, 2008 1 #3 msquared48 Structural Joined Aug 7, 2007 Messages 14,745 Location US The APA (American Plywood Association) has a lot of information on built-up plywood members, with design examples. I would start by googling there. Mike McCann McCann Engineering Upvote 0 Downvote
The APA (American Plywood Association) has a lot of information on built-up plywood members, with design examples. I would start by googling there. Mike McCann McCann Engineering
Jan 14, 2008 #4 Einsteim Structural Joined Jan 10, 2008 Messages 76 Location US It really depends on the "repair" that is required. It may need to be reinforced with steel plates or angles. Or sistered with engineered wood members. Upvote 0 Downvote
It really depends on the "repair" that is required. It may need to be reinforced with steel plates or angles. Or sistered with engineered wood members.