1
- #1
redoak52
Mechanical
- Feb 23, 2004
- 3
We have 6 inch dia. spiral welded steel columns in our warehouse that have received repeated hits from lift trucks. The bottom 24 in. of the column has been pushed inward or essentially the side of the column has been flattened inward toward the centerline of the column. Can someone recommend a repair method?