Hi everyone,
I am looking to substitute EPT rubber gasket with SS304 spiral wound gasket (with 99.5% graphite filling) on all piping flanged connections. I have read that there are quite a few cases of buckling of the metal winding and then finding their way into the piping. I was looking for some oprtational feedback or information on failures of this type. I am not sure if I should specify inner ring for these spiral wound graphite filled gaskets.
All feedback welcome.
Regards
I am looking to substitute EPT rubber gasket with SS304 spiral wound gasket (with 99.5% graphite filling) on all piping flanged connections. I have read that there are quite a few cases of buckling of the metal winding and then finding their way into the piping. I was looking for some oprtational feedback or information on failures of this type. I am not sure if I should specify inner ring for these spiral wound graphite filled gaskets.
All feedback welcome.
Regards