BSS 1452 Class 17

Status
Not open for further replies.

tejas1

Mechanical
Jun 8, 2004
17
I need to do a thickness calculation on a dryer roll which was manufactured in the U.K. by Black and Clawson in 1975.

The nameplate is stamped TS=35000psi.

The material is BSS 1452 Class 17. Does anyone know if there is an ASME equivalent for this material?

Thanks in advance.
 
Replies continue below

Recommended for you

BS 1452 is a Grey Cast Iron. Look at ASME SA-278 and check stress values. ASTM A278,48
 