Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JAE on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

BS S 130 Stainless Steel 1

Status
Not open for further replies.

GaryJ

Materials
Joined
Nov 15, 2001
Messages
4
Location
GB
Can anyone help me find the relevant spec or werkstoff number relating to BS S 130 Stainless Steel?
Is this an aircraft grade steel?

The material is used to manufacture rivets.

Thanx in advance :)
 
Yes, it is a aircraft grade - a variation of type 347 stainless steel.

S130 - 0.08% max C, 0.20-1.00 % Si, 0.50-2.00% Mn, 0.035 % P, 0.025 % S, 17.00-19.00 % Cr, 8.00-11.00 % Ni, 10xC min Nb, other Mo

Similar metals

347-S17 (EN58 F/G)
AFNOR Z26CNNb 18-11
AISI 347/ SAE 30347
AMS 5646
MIL-S-862B 347
MIL-S-27419 347
WS 1.4550 XCrNiNb18 9
 