Dear All,
Can anyone tell me where to find information regarding this material e.i. Yield Strength at certain temperature or the allowable stress. I mean not from the code book. Thanks a lot!!
 
What do you mean by "not from the code book"?

To get the physical properties you should look in the code book, i.e EN 10028-6 (may be preceeded by BS, DIN etc)

To get the design stresses you should calculate those from the physical properties in accordance with the design code which in your case is probably EN13445 (the new european pressure vessel code) or perhaps EN13480 (the new european piping code)

I don't have a copy of EN10028-6, but I had a look in the Stahlschlüssel (german "key to steel" bible) - the material was listed but without physical properties.

You may anyway find use of the information that was there, including a supplier:

Search for P500QL2:
*************************************
Material Number
1.8865

Steel group
Alloy special steels: High strength weldable structural steels, steels not intended for heat treatment by user

Symbol
P500QL2

Standards
DIN EN 10028-6
(02/97) Flat products made of steel for pressure purposes. Weldable fine grain steels, quenched and tempered.
International conformity
EN 10028-6 (96)

Supplier:
********************************************
Aktiengesellschaft der Dillinger Hüttenwerke,
Postfach 15 80; 66748 Dillingen/Saar,
Tel.: (0 68 31) 47-0, Telex: 4 43 711-0 dhd, Fax: (0 68 31) 47-22 12,
E-Mail: info@dillinger.de
**********************************************

You can buy the british EN standards at
Other european versions available via

Hope this helps
Regards
Mogens
 
Thanks for the reply.
Currently, I try to get EN 10028 part 1~6 but haven't get approval from our management (we are more on ASME). I have a verry urgent job to bid. So, to get information from code book is not an option to me, at least for the time being. Anyway, thanks again and hope that you understand.
 
Found this on the web searching P500QL2:


You might be able to find some material strengths in this document.

The design stress for steels (other than Austenitic SS) according to EN13480:

The smaller of:
Yield Strength at Temperature/1.5 or
Tensile strength /2.4

regards
Mogens
 
To hockchong
Hi!!
Probably I have some bits here!!
Please send me your e-mail
noaminfa@wanado.nl
 