Morning all;
I hope someone can help who is in the know. I have been looking at a number of 3.1 mill certificates against a BOM and found an issue (I think).

The material requested is S355JR+N but on the material certificate it just says S355JR. I have queried this back to the supplier and they said not all mills state the +AR or +N. Is this correct? I would assume if you ask for +N or +AR it should state it on the mill cert?

Hope someone can help?
Regards,
Ant
 
Replies continue below

Recommended for you

It is mandatory to indicate the delivery condition in the inspection document, see BS EN 10025-2 subclause 6.3
"If an inspection document is required (see 8.2) the delivery condition shall be indicated in it with its specific symbol (+N, +AR or +M). In case the products are ordered in the delivery condition +N, +AR or +M the specific symbol (+N, +AR or +M) shall be added to the designation (see 4.2.2).
 
If the certificate states that the material has been normalized, it is ok.
 