Any problem to use a BS holding down anchor bolt (or threaded rod to BS standard BS 7419) with ASTM Nut(ASTM A563)? Thank u
 
Replies continue below

Recommended for you

ASTM A 563M nuts should be compatible regarding material strength.

You need to review the thread dimensions for both parts to make sure they are compatible. The anchor bolts are made to loose tolerances, while the nuts may or may not be.
 