Can anyone recommend a good reference source, where I can find information on bronze bushing design?
I have an application with (4) four 158" DIA sheave with a pressed-in bronze bushing, rotating on a steel shaft. One sheave is fixed and the remaining (3) three are floating. The problem is with the recommended operating clearances (max, min)? The sheaves were purchased about 10 years ago and there is very little information available and the supplier is not willing to give out any recommended running clearances or original (as purchased) clearances. The operating parameters are as follows:
RPM - 90 max
Sheave Weight - 5000lb
Applied Load - 14,000 lb
Shaft OD - 9in to 11in (Can't measure directly)
Bushing Material - SAE 65, Bronze (Best Guess)
Shaft Material - 4140 (Best Guess)
Lubrication - Synthetic Grease
Any help or additional insights are appreciated.
I have an application with (4) four 158" DIA sheave with a pressed-in bronze bushing, rotating on a steel shaft. One sheave is fixed and the remaining (3) three are floating. The problem is with the recommended operating clearances (max, min)? The sheaves were purchased about 10 years ago and there is very little information available and the supplier is not willing to give out any recommended running clearances or original (as purchased) clearances. The operating parameters are as follows:
RPM - 90 max
Sheave Weight - 5000lb
Applied Load - 14,000 lb
Shaft OD - 9in to 11in (Can't measure directly)
Bushing Material - SAE 65, Bronze (Best Guess)
Shaft Material - 4140 (Best Guess)
Lubrication - Synthetic Grease
Any help or additional insights are appreciated.