Hello. Does anyone know of a formula/advice for the pressing in of a sintered bronze bearing into steel or aluminum - in so much as not effecting the ID of the bearing, but still keeping a press fit? Thank you.

Semtorq
 
Replies continue below

Recommended for you

Lame's Equation can be used, which is an alternate form of the Von Mises-Hencky Equation for Thick Walled Pressure Vessels. You can find several websites by search under those key words.

Also, the University of Tennessee does an excellent job with an Advanced Mechanical Engineering lecture on this subject. The notes are complete with equations and a worked example.

Kenneth J Hueston, PEng
Principal
Sturni-Hueston Engineering Inc
Edmonton, Alberta Canada
 
Machinery's Handbook has some simplified formulas that can be helpful.

In general, and especially for thin bushings, it's not possible to get a press fit on the o.d. that does not also alter the i.d.