We are looking to replace some titanium and stainless parts with a lower cost / easier to source material and I was exploring 651 silicon bronze, aluminum bronze, and 70-30 and 90-10 copper nickel alloys. There are two applications that are of primary importance:
(1) a lead screw (30 PSI tensile/compression) exposed to salt spray.
(2) a stationary non-structural piece (electronic housing).

The screw can have anode protection installed but the electronic housing cannot (limited exposed surface). On the latter the reduction of bio-fowling is as important as corrosion as this is a set and forget device. Any suggestions based on experience and costs?

thanks
 
Replies continue below

Recommended for you

If you really want seawater resistance you are looking at NiAlBronze or 70/30. The other alloys will sort of work, but nothing like a 6% Mo stainless or Ti.

You won't save much money. One advantage of the Cu based alloys is the biocide effect. As long as you are allowed to have a release of Cu ions you can take advantage of this.

= = = = = = = = = = = = = = = = = = = =
Corrosion, every where, all the time.
Manage it or it will manage you.
 
any particular grade of Ni Al Bronze? I was looking at C62300 and C95500 initially.
 