I am interested in anyone's experience in broaching ETD 150. The broach would be between a 3/8" - 1/2" Hex by 1/2" deep. Material hardness of ETD 150 may pose difficulties in broaching, but I am not sure as it seems to be on the edge. Does anyone have any experience?

Pete
 
Replies continue below

Recommended for you

It will be similar to 4140 HT. Slower speeds, shorter depths of cut, and a good setup will provide success
 