I have a question with regard to brittle fracture and design of steel stacks. In pressure vessels we must consider the minimum design metal temperature and determine if the material selected is suitable for this temperature so that brittle fracture will not occur. However, my understanding of brittle fracture is that it only occurs as a result of primary membrane stress. Since the stresses on stacks are usually secondary bending stresses, is brittle fracture a concern?