Is anybody aware of a reference (e.g. codes, specs, etc....) detailing the limit of 50 N/mm2 of membrane stress as the limit for brittle fracture?
 
Replies continue below

Recommended for you

Part 3 of API 579/ASME FFS-1 references a 55 MPa limit for when brittle fracture can be a concern for carbon and low alloy steels.
 