Does anybody know where I can find the American Spec (AISI?) equivalence of the British Spec S99?
S99 chemistry: 0.36-0.44 C, 0.1-0.35 Si, 0.45-0.70 Mn, 0.025 P max, 0.020 S max, 0.50-0.80 Cr, 0.45-0.65 Mo, 2.30-2.80 Ni, Fe balance.
If there is no equivalent, does anybody know the embrittlement relief time and temperature of S99 as well as tensile strength?
Thank you,
Coka
S99 chemistry: 0.36-0.44 C, 0.1-0.35 Si, 0.45-0.70 Mn, 0.025 P max, 0.020 S max, 0.50-0.80 Cr, 0.45-0.65 Mo, 2.30-2.80 Ni, Fe balance.
If there is no equivalent, does anybody know the embrittlement relief time and temperature of S99 as well as tensile strength?
Thank you,
Coka