Any suggestions on how to keep the cannonballs from corroding on exposure to air?
From the BBC:
The Mary Rose sank in 1545 and was raised from the sea in 1982. The cannonballs on board are difficult to conserve because chlorine has got into them from being in the sea. The chemical has got in all the way to its core. This means that they start to corrode if they are exposed to the air.
Dr Schofield's team has tried to remove the chlorine by soaking some cannonballs in solution. But the researchers found that although they had extracted some they hadn't removed it all. They discovered this when the cannonballs began to disintegrate when they were put on display.
Dik
From the BBC:
The Mary Rose sank in 1545 and was raised from the sea in 1982. The cannonballs on board are difficult to conserve because chlorine has got into them from being in the sea. The chemical has got in all the way to its core. This means that they start to corrode if they are exposed to the air.
Dr Schofield's team has tried to remove the chlorine by soaking some cannonballs in solution. But the researchers found that although they had extracted some they hadn't removed it all. They discovered this when the cannonballs began to disintegrate when they were put on display.