alloyboy
Structural
- Feb 11, 2003
- 13
I am fabricating a few items using 1/8 alum. diamond plate.
I used a plasma torch to cut the pieces out and welded them
using the TIG process. My question is; how to get the luster
back in the cut/weld area.
I have seen pickup toolboxes made from this material, and
the weld areas are as shiny as the panels.
Thanks, alloyboy
I used a plasma torch to cut the pieces out and welded them
using the TIG process. My question is; how to get the luster
back in the cut/weld area.
I have seen pickup toolboxes made from this material, and
the weld areas are as shiny as the panels.
Thanks, alloyboy