3
Concerning Heater tubes, are there acceptable Brinell hardenss limits, high and low for safe operation.
I would like to know the acceptable high and low limits or good Engineering practice for 1.25cr, 5 cr and 9 cr tubes in refinery service. Any help would be appreciated, thanks.
 