I've done a little searching but not come to a comprehensive answer so I'm asking for some help.
We currently have a standard note:
ELECTROLESS NICKEL PLATE, .0003-.0005 THICK IN ACCORDANCE WITH SPEC MIL-C-26074 OR EQUIVALENT. DIMENSIONS APPLY AFTER PLATING.
My manufacturing engineering manager just asked that I split the note into 2 flavors for aesthetic reasons.
BRIGHT ELECTROLESS NICKEL PLATE, .0003-.0005 THICK IN ACCORDANCE WITH SPEC MIL-C-26074 OR EQUIVALENT. DIMENSIONS APPLY AFTER PLATING.
DULL ELECTROLESS NICKEL PLATE, .0003-.0005 THICK IN ACCORDANCE WITH SPEC MIL-C-26074 OR EQUIVALENT. DIMENSIONS APPLY AFTER PLATING.
I'm concerned this isn't anywhere near properly specifying the distinction.
(I'm OK with accepting the Mil std listed is obsolete which is why we have the 'or equivalent'. We aren't ISO9001 or anything so that aspect isn't too much of an issue. Although if this directly relates to bright V Dull I'm OK with looking at changing it)
I was thinking ‘bright’ or ‘dull’ would relate to a class, type or grade or something.
Any help on how to more properly specify this is appreciated, thanks.
We currently have a standard note:
ELECTROLESS NICKEL PLATE, .0003-.0005 THICK IN ACCORDANCE WITH SPEC MIL-C-26074 OR EQUIVALENT. DIMENSIONS APPLY AFTER PLATING.
My manufacturing engineering manager just asked that I split the note into 2 flavors for aesthetic reasons.
BRIGHT ELECTROLESS NICKEL PLATE, .0003-.0005 THICK IN ACCORDANCE WITH SPEC MIL-C-26074 OR EQUIVALENT. DIMENSIONS APPLY AFTER PLATING.
DULL ELECTROLESS NICKEL PLATE, .0003-.0005 THICK IN ACCORDANCE WITH SPEC MIL-C-26074 OR EQUIVALENT. DIMENSIONS APPLY AFTER PLATING.
I'm concerned this isn't anywhere near properly specifying the distinction.
(I'm OK with accepting the Mil std listed is obsolete which is why we have the 'or equivalent'. We aren't ISO9001 or anything so that aspect isn't too much of an issue. Although if this directly relates to bright V Dull I'm OK with looking at changing it)
I was thinking ‘bright’ or ‘dull’ would relate to a class, type or grade or something.
Any help on how to more properly specify this is appreciated, thanks.