For brazer performance, Section IX QB-302.1 requires testing of the braze coupon in accordance with QB-452. The right hand column of Table QB-452.1 requires 2 "Peel or Section" specimens. Previous practice at a manufacturer's plant has been to always perform section tests. However, Note 1 of the table says "Sectioning tests may be substituted for the peel test when the peel test is impractical to perform (e.g. when the strength of the brazing filler metal is equal to or greater than the strength of the base metals)".
Does this note imply that peel testing is always required except when the strength situation makes it impractical, or is it really just advising not to try peel tests for that situation, and section tests are always acceptable?
I haven't been able to find any interpretations on the issue.
Does this note imply that peel testing is always required except when the strength situation makes it impractical, or is it really just advising not to try peel tests for that situation, and section tests are always acceptable?
I haven't been able to find any interpretations on the issue.