trying to manufacture braided pebax tubing w ptfe inner layer. Having a hard time keeping one of braid square during assembly. Ptfe layer extends past braid on that end. Hence cannot square cut. Anyone with braided tubing manufacturing experience using heat shrink, please suggest any tips.
 