rakucheleri
Mechanical
Dear Experts,
This is my first time repairing a open top Floating roof ,Double Deck storage tank designed according to API 650 for Oil Storage., date of fabrication is 1999, this tank suffers from heavily corrosion in Entire bottom plates (according to the inspection report, Entire bottom plates are set to be changed , No changes for annular plates). in order to do that , i am going to use gas cutting technique to remove the plates. Once these plates are removed and before welding the new ones, the tank shell may suffer buckling due to its weight.ck
Tank dimensions : 65 Mtr Dia x 20 Mtr Ht x Double deck floating roof tank
First Shell course Thk : 32 mm
Material of construction : IS 2062
Bottom Plate Thk : 8 mm
Annular Plate Thk : 14 mm
Deck Weight : 400 Ton
Shell Weight : 1000 Ton approx
Roof Legs : placed 5 mtrs apart from each other x 151 Nos x 3" sch 80
looking for recommendations and comments for
1) how to change entire bottom plate except annular plate
2) How to control Buckling/mechanical distortions due to shell weight
3) how to remove plate when deck is in Top leg position
4) how many area can be removed at a time
5) How & Where to do cutting on shell for removal /entry for bottom plates
6) is PWHT is required for shell openings.
all feedback is always welcome
thank you in advance
This is my first time repairing a open top Floating roof ,Double Deck storage tank designed according to API 650 for Oil Storage., date of fabrication is 1999, this tank suffers from heavily corrosion in Entire bottom plates (according to the inspection report, Entire bottom plates are set to be changed , No changes for annular plates). in order to do that , i am going to use gas cutting technique to remove the plates. Once these plates are removed and before welding the new ones, the tank shell may suffer buckling due to its weight.ck
Tank dimensions : 65 Mtr Dia x 20 Mtr Ht x Double deck floating roof tank
First Shell course Thk : 32 mm
Material of construction : IS 2062
Bottom Plate Thk : 8 mm
Annular Plate Thk : 14 mm
Deck Weight : 400 Ton
Shell Weight : 1000 Ton approx
Roof Legs : placed 5 mtrs apart from each other x 151 Nos x 3" sch 80
looking for recommendations and comments for
1) how to change entire bottom plate except annular plate
2) How to control Buckling/mechanical distortions due to shell weight
3) how to remove plate when deck is in Top leg position
4) how many area can be removed at a time
5) How & Where to do cutting on shell for removal /entry for bottom plates
6) is PWHT is required for shell openings.
all feedback is always welcome
thank you in advance