I am new to injection-molded parts. I have read some online available guide sources on injection-molding process. All guide sources recommends using Boss thickness from 60-80% of the Wall thickness i.e. if Wall thickness is 4mm then 2.4 to 3.2mm for the Boss thickness.
I am not able to decide that if Boss thickness of the 6mm is used for a Wall thickness of 4mm: Is injection-molded process feasible for the part? Any recommendation on this topic would be appreciated.
Thanks
I am not able to decide that if Boss thickness of the 6mm is used for a Wall thickness of 4mm: Is injection-molded process feasible for the part? Any recommendation on this topic would be appreciated.