Could you give me the name of the best known Book about.
STAMPING CUTING FORMING SHEET METALS BY DIE on press .
Pardal
 
Replies continue below

Recommended for you

Books to consider:

1. ASM HANDBOOK Volume 14 Forming and Forging. You can obtain this at
2. Design Guidelines for Precision Metal Stampings and Fabrications from the Precision Metalforming Association. Website is
A great website for information on steel stamping materials, design practices, etc. is the Auto Steel Partnership, There is a huge collection of free material on this site. Another good website is for the PMA I mentioned above: They have an online version of their monthly magazine Metalforming available there.
 
Hi TVP
thanks again for your help.

Pardal
 