I HAVE AN ORDER FROM MY CLIENT FOR 4" GLOBE VALVE CLASS 300 TRIM 1 AND THE SPECIFICATION MENTIONS THE BELOW REQUIREMENT:

BONNET GASKET, DOUBLE JACKETED WITH MIN. 95% PURITY GRAPHITE FILLED.

MY SUPPLIER IS OFFERING STANDARD SS304+GRAPHITE FOR THE BONNET GASKET. CAN ANY ONE ADVISE.
 
Get a new supplier.

Patricia Lougheed

******

Please see FAQ731-376: Eng-Tips.com Forum Policies for tips on how to make the best use of the Eng-Tips Forums.
 
pennpiper (Mechanical),

I am not yelling. I am just asking suggestions from expert like you. I tried with many suppliers but they have informed that BONNET GASKET, DOUBLE JACKETED WITH MIN. 95% PURITY GRAPHITE FILLED is not in their scope of manufacturing. All of them offer SS304+GRAPHITE.

I have a doubt whether Double jacket gasket is out dated & SS304+Graphite is the latest technology. My client has no idea about his exact requirement. Therefore, I want to get advise from experts like you. If Double jacket gasket is out dated & if no body is manufacturing that, them I can inform my client accordingly & get his approval. Please give me your valuable advise. I am not an expert in valve, I am just a beginner.
 
Using capitals is yelling (standard internet protocol). Where are you located and how far a field of suppliers are you searching?
 
Dear cloa,

I am in the Middle-East. I have a list of approved manufacturers in Europe & Asia. I contacted them & they are unable to manufacture the required BONNET GASKET, DOUBLE JACKETED WITH MIN. 95% PURITY GRAPHITE FILLED. All of them offer SS304+GRAPHITE.

I have a doubt whether Double jacket gasket is out dated & SS304+Graphite is the latest technology. My client has no idea about his exact requirement. Therefore, I want to get advise from experts like you. If Double jacket gasket is out dated & if no body is manufacturing that, them I can inform my client accordingly & get his approval. Please give me your valuable advise. I am not an expert in valve, I am just a beginner.
 
I don't think "double jackets" are out-dated as there are still manufacturers that offer double jacket gaskets. I would suggest googling on the words "double jacket graphite valve gasket" and then calling some of the manuafacturers whose sites come up to discuss your specific needs.

Patricia Lougheed

******

Please see FAQ731-376: Eng-Tips.com Forum Policies for tips on how to make the best use of the Eng-Tips Forums.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top