This is a common practice. Contact your TPE supplier for details. GLS is a TPE supplier I used to work for and they did this many times for their clients. Some TPE's require a primer to get good ahesion to steel. Lord Chemical in Erie PA is a good supplier of these primers. ChemLock and Chem Grip are two of their trade names.