Apr 14, 2009 #1 ericlast Industrial Joined Apr 14, 2009 Messages 1 Location US I need to bond a Mertex (polyurethane) liner of a lay-flat fire hose to some heat-shrink (polyolefin). Does anyone know an adhesive that will work? Thanks in advance.
I need to bond a Mertex (polyurethane) liner of a lay-flat fire hose to some heat-shrink (polyolefin). Does anyone know an adhesive that will work? Thanks in advance.
Apr 20, 2009 #2 unclesyd Materials Joined Aug 21, 2002 Messages 9,819 Location US I would give these people a call. http://www.reltekllc.com/index.html Upvote 0 Downvote