I need to bond a thin metal wires into a porous plastic cylinders made from PE or PP. The metal wire should come right out of the side of the cylinder and it should be always at the same position. The cylinder has diameter of 2 mm. The metal wire has diameter of 0.1 mm.
I was thinking of drilling a hole (e.g. with laser) through the cylinder and then welding the wire from the other side to the side of the cylinder. However I don't know how ultrasonic or laser welding works with porous plastics. I can have use different wire forms (e.g. hooks) but the wire should be thightly attached to the cylinder.
Does anyone have experience in joining parts to porous plastics?
I was thinking of drilling a hole (e.g. with laser) through the cylinder and then welding the wire from the other side to the side of the cylinder. However I don't know how ultrasonic or laser welding works with porous plastics. I can have use different wire forms (e.g. hooks) but the wire should be thightly attached to the cylinder.