Hello,

what material should be used to bond ceramic tiles to carbon steel plate and should be also suitable to stand high temperature at the opposite side of the carbon steel plate.
please indicate the bond material composition since trade names differ from country to country.

regards,
roker
 
Replies continue below

Recommended for you

You need to comeback with more details like what type ceramic (size and thickness), temperature, cyclic service?, surface area, and anything else that might help.
 
hello unclesyd,

the ceramic tiles are 5x5 cm 5 mm thick, temperature about 250 deg C, continuous service, the metal is carbon steel.

regards,
roker
 
It may be that the temp spec'd is high. Anyway, here are some links, maybe a phone call will get you going in a direction?

Code:
[URL unfurl="true"]http://www.laticrete.com/techdata/tds146.pdf[/URL]
[URL unfurl="true"]http://ramenterprise.thomasnet.com/item/enecon/eneclad-174-super-bond/eneclad-superbond?&forward=1[/URL]
[URL unfurl="true"]http://www.elichem.co.uk/plantmaint.htm[/URL]
[URL unfurl="true"]http://www.tileusa.com/ANSIA108/images/A108.01.pdf[/URL]

==========================================