Hi All,
I am working on a project looking at either using a bolted steel tank ( similar to API 12D/F, etc) vs a API650 Welded tank. I am looking for advice from people on the maintenance differences, if it is worth doing the Bolted steel tank over the Welded tank? In my own opinion I want to have a welded Tank to API 650 since the current tanks have been in operation for >25 yrs and have not had any issues, but the price difference is making it difficult to justify.
Tank Details:
Size: 950m3
Contained Liquid: Demineralised water with a high oxygen content
purpose: Demineralised water for a 12,000 kPag HP boiler circuit ( through deaerator to remove oxygen)
Pressure: head pressure only from the water
Design Temperature : 70 deg C
Options
Bolted Steel tank :
- Mild steel shell
- internal liner ( lifetime 10 yrs)
installed cost $250,000
Welded API 650 tank:
- 304 SS
installed cost of $650,000
Any help is appreciated.
I am working on a project looking at either using a bolted steel tank ( similar to API 12D/F, etc) vs a API650 Welded tank. I am looking for advice from people on the maintenance differences, if it is worth doing the Bolted steel tank over the Welded tank? In my own opinion I want to have a welded Tank to API 650 since the current tanks have been in operation for >25 yrs and have not had any issues, but the price difference is making it difficult to justify.
Tank Details:
Size: 950m3
Contained Liquid: Demineralised water with a high oxygen content
purpose: Demineralised water for a 12,000 kPag HP boiler circuit ( through deaerator to remove oxygen)
Pressure: head pressure only from the water
Design Temperature : 70 deg C
Options
Bolted Steel tank :
- Mild steel shell
- internal liner ( lifetime 10 yrs)
installed cost $250,000
Welded API 650 tank:
- 304 SS
installed cost of $650,000
Any help is appreciated.