I am in a confusing predicament with bolt torques and bolt yield assessments. We are reviewing a new software for gasket assessment of seating stresses etc. It is quite good in that it enables us to insert different bolt yields from test certificates and then assess the effective seating stress for the gasket based on different torque values.
However, a senior engineer in another department has rubbished the software as he insists that the ability of a bolt to stretch under torque is purely dependant upon the modulus of elasticity and not the physical yield as shown on the material test certificate.
In summary, I need to assess if my thinking is wrong. I have, up until this moment, worked on the basis that a bolt with a higher yield will enable a higher torque to be delivered and thereby deliver a greater seating load. However, if i consider the other engineers assessment then yield should not have any part to play.
Any assistance or help that folks could offer would be of great help.
Many thanks
I am in a confusing predicament with bolt torques and bolt yield assessments. We are reviewing a new software for gasket assessment of seating stresses etc. It is quite good in that it enables us to insert different bolt yields from test certificates and then assess the effective seating stress for the gasket based on different torque values.
However, a senior engineer in another department has rubbished the software as he insists that the ability of a bolt to stretch under torque is purely dependant upon the modulus of elasticity and not the physical yield as shown on the material test certificate.
In summary, I need to assess if my thinking is wrong. I have, up until this moment, worked on the basis that a bolt with a higher yield will enable a higher torque to be delivered and thereby deliver a greater seating load. However, if i consider the other engineers assessment then yield should not have any part to play.
Any assistance or help that folks could offer would be of great help.