Bolts is K-monel, QQ-N-286E, (Cold Drawn and age hardened)UTS/YS=140/100 ksi
Set End is Monel, QQ-N-281D Amd 2, Class A Annealed) UTS/YS= 70/25 ksi
Length of Engagement is .44 inch
Per FED-STD-H28/2B:
"If failure of a fastening system using standard threaded fasteners should occur it is generally more economical that the externally threaded part will break rather than that either the external or internal thread will strip. In other words, the length of thread engagement should be sufficient to develop the full strength of the screw. Thus, the length of internal thread and the dimensions of this thread, particularly its minor diameter, should be such that, taking into account a possible difference in strength of material of the internal and external threads, the threaded portion of the externally threaded part will break before either the external or internal threads strip. Due to this situation, lengths of engagement formulas are derived from shear formulas with tensile stress area AS replaced by 2AS because the required area in shear is twice the tensile stress area in order to develop the full strength of the externally threaded part. This relationship is based upon experiments made by the National Bureau of Standards in 1929, in which it was found that for hot-rolled and cold-rolled steel, and brass screws and nuts, this factor varied from 1.7 to 2.0. The effect of combined stress is not taken into account in calculation of LE because the added shear load affects both tensile and shear stresses in approximately the same proportion."