I have a problem involving determination of proper torque using 3/8-24UNF K-monel 100ksi YS bolts into a Monel 25K YS plate. It is generally desired that the externally threaded part will break before the external or internal threads slip. FED-STD-H28/2B accounts for this by ensuring adequate Length Engagement. In my case I have .44 inch which is more than the .391 required by H28/2B. When using PCBolts software program, if you let it calculate everything it comes up with a required torque of 14ft-lbs based on limiting the YS in the set end to 2/3 of YS(25ksi). If you plug in a required preload 4640lbs(.60 YS of the bolt) then it gives a torque of 22ft-lbs. I believe to latter is correct. Any thoughts?