Jasmine55
Petroleum
- Oct 26, 2014
- 3
Hello Members,
This may be a stupid question.
Under sized bolts are used in some of the piping systems as follows,
16" - 300# flange
Used bolt size: 1 1/8"
As per ASME: 1 1/4"
The design pressure of the piping system is 25bar.
We found this discrepancy at the later stage of the project and changing now is huge task since the scaffolds and other resources are already demobilized.
Could any of the member ever came like this situation and what was the final decision made?
Is there any deviation/tolerance in ASME codes?
Thanks for your valuable feedback.
This may be a stupid question.
Under sized bolts are used in some of the piping systems as follows,
16" - 300# flange
Used bolt size: 1 1/8"
As per ASME: 1 1/4"
The design pressure of the piping system is 25bar.
We found this discrepancy at the later stage of the project and changing now is huge task since the scaffolds and other resources are already demobilized.
Could any of the member ever came like this situation and what was the final decision made?
Is there any deviation/tolerance in ASME codes?
Thanks for your valuable feedback.