Refer to NACE MR0175, acceptable bolt material for H2S service is A193-B7M.
In case of high temperature, A193-B16 should be better for strength concern. However, A193-B16 is not indicated in NACE MR0175.
Which is suitable material for high temperature and H2S service? Please comment.
In case of high temperature, A193-B16 should be better for strength concern. However, A193-B16 is not indicated in NACE MR0175.
Which is suitable material for high temperature and H2S service? Please comment.