Has anyone ever come up with the situation where you have steel coming from over seas with metric bolt holes and the design was for imperial bolts? My question, the holes for 3/4" A 325 bolts in a bearing connection are 22mm (7/8") where by code they should be 21.4mm(13/16"). An oversize hole is 24mm (15/16")Is this an acceptable for a bearing connection?
Has anyone ever come up with the situation where you have steel coming from over seas with metric bolt holes and the design was for imperial bolts? My question, the holes for 3/4" A 325 bolts in a bearing connection are 22mm (7/8") where by code they should be 21.4mm(13/16"). An oversize hole is 24mm (15/16")Is this an acceptable for a bearing connection?