Greetings,
I was reviewing a piping specification for high temperature austenitic stainless steel operating at 1200 deg F [635 deg C].But the operating pressure is low [1 kg/cm2]. The metallurgy for the bolt material specified is SB 408 UNS N08811. This bolt material is not listed in [Design stress values for bolting material] Table-A2 of ASME B31.3. But I found the stress values in Table A-1. But it cannot be used for bolting.
My understanding is, for bolting higher yield strength is required. The yield strength and creep strength of SB 408 UNSN08811 is not encouraging [atleast when compared to B8T,B8M or B8C].Even though the pressure is very low this may under go stress relaxation and loose the clamping force.
When I consider SA 453 GR 660B which is having higher yield strength & creep strength and matches the thermal co-efficient of expansion of Aus. Stainless steel. But the stress values are available only up to 1050 deg F [due to heat treatment it undergoes].
Any body using SB 408 UNSN08811 / SA 453 GR 660B for Temperature above 600degC? Please share your experience..
I was reviewing a piping specification for high temperature austenitic stainless steel operating at 1200 deg F [635 deg C].But the operating pressure is low [1 kg/cm2]. The metallurgy for the bolt material specified is SB 408 UNS N08811. This bolt material is not listed in [Design stress values for bolting material] Table-A2 of ASME B31.3. But I found the stress values in Table A-1. But it cannot be used for bolting.
My understanding is, for bolting higher yield strength is required. The yield strength and creep strength of SB 408 UNSN08811 is not encouraging [atleast when compared to B8T,B8M or B8C].Even though the pressure is very low this may under go stress relaxation and loose the clamping force.
When I consider SA 453 GR 660B which is having higher yield strength & creep strength and matches the thermal co-efficient of expansion of Aus. Stainless steel. But the stress values are available only up to 1050 deg F [due to heat treatment it undergoes].
Any body using SB 408 UNSN08811 / SA 453 GR 660B for Temperature above 600degC? Please share your experience..