Hi sdz,
I'd classify that as a machine flame-cut edge, flame essentially referring to the heat involved with the edge preparation, and there is significant heat involved with laser-cutting. This ought to typically result in edge distance of 1.50 df as per relevant table in AS 4100 Section 9.
Tom