DWHA
Structural
- Jan 31, 2007
- 315
Different edge distances are allowed depending on what type of edge is present on the steel (per AISC, AASHTO, AREMA, etc.). There are 2 classes, 1 is rolled or thremally cut, the other is sheared. My question is what about edges that have been sawed. To me sawing steel would be the same as rolled and thermally cut because the damage to the steel is not like when the steel is sheared, but that is just my guess. What do others allow/think......