We have a 30MVA, 132/33KV Transformer that was removed from service due to leakage, for about 3years and the oil was beign removed and used elsewhere. Recently, the leakages were sealed and it was filled with oil and energised without picking any load for five days. On the fifth day the primary breaker triped due to a fault on another transformer sharing the same primary breaker.
After clearing the fault the two transformers were restored, but this very transformer started making a noise as if something is boiling inside and after some time it made a big bang noise with the whole trasformer vibrating. When bleeded a white gas like steam was coming out. What could the cause.
We have no means of testing the gas, please.
After clearing the fault the two transformers were restored, but this very transformer started making a noise as if something is boiling inside and after some time it made a big bang noise with the whole trasformer vibrating. When bleeded a white gas like steam was coming out. What could the cause.
We have no means of testing the gas, please.